Bundled alloy pipe in storage

Pipe

Seamless and welded pipe in copper, copper-nickel, marine grade aluminium, high nickel alloys and stainless steel.

Bundled alloy pipe in storage

Overview

Pipe in five material families

We supply seamless and welded pipe and tube across five material families, from commercially pure copper through to high nickel alloys. Marine grade aluminium is stocked for shipbuilding and offshore work.

Sizes, schedules, lengths and end finish are confirmed against each enquiry.

Specifications

Product specifications

The range we quote against. Anything outside this is worth asking about — we will confirm on enquiry.

Specifications
ItemDetail
Product formsSeamless pipe, Welded (ERW / EFW) pipe, Tube, Coil
Size range1/2" to 24" NB (larger on enquiry)
Wall thicknessSCH 5S, 10S, 40S, 80S, 160, XXS
LengthSingle random, double random or cut to length
Stainless standardASTM A312 / A358
Nickel alloy standardASTM B161 / B165 / B167 / B407 / B423 / B444
Copper & cupro-nickel standardASTM B88, ASTM B466 / B467
Aluminium standardASTM B241 / B210
EndsPlain, bevelled or threaded
DocumentationMill test certificate as agreed at order stage

Indicative data only. Values are typical for the grade and are shown for guidance. Confirm the applicable standard, and the actual figures on the mill test certificate, before using them for design or procurement.

Grades & Materials

Materials we supply

Each material family below is offered across the full product range.

Copper

Copper pipe and tube for plumbing, refrigeration, heat transfer and electrical work.

  • Copper C10200 (OFC)
  • Copper C11000 (ETP)
  • Copper C12200 (DHP)

Standards: ASTM B88, ASTM B42, ASTM B280

Copper-Nickel

The standard seawater piping material, also used in condenser and heat exchanger tube.

  • Cupro-Nickel 90/10 (C70600)
  • Cupro-Nickel 70/30 (C71500)

Standards: ASTM B466 (seamless), ASTM B467 (welded), ASTM B111 (tube)

Aluminium Marine Grade

Marine grade aluminium pipe for shipbuilding, offshore structures and boatbuilding.

  • Aluminium 5083
  • Aluminium 5086
  • Aluminium 6061
  • Aluminium 6063

Standards: ASTM B241, ASTM B210

High Nickel Alloys

For the most demanding corrosive and high-temperature lines.

  • Inconel 600 / 625
  • Incoloy 800 / 825
  • Monel 400
  • Nickel 200 / 201
  • Hastelloy C-276

Standards: ASTM B161 / B165 / B167 / B423 / B444

Stainless Steel

The general-purpose range in austenitic, stabilised and duplex grades.

  • SS 304 / 304L
  • SS 316 / 316L
  • SS 321
  • SS 347
  • Duplex 2205

Standards: ASTM A312, ASTM A358, ASTM A790 (duplex)

Dimension Chart

Dimensions

Standard pipe sizes — outside diameter and SCH 40 wall thickness
Nominal sizeNB (mm)Outside diameter (mm)SCH 40 wall (mm)
1/2"1521.32.77
3/4"2026.72.87
1"2533.43.38
1-1/4"3242.23.56
1-1/2"4048.33.68
2"5060.33.91
3"8088.95.49
4"100114.36.02
6"150168.37.11
8"200219.18.18
10"250273.09.27
12"300323.810.31

Indicative data only. Values are typical for the grade and are shown for guidance. Confirm the applicable standard, and the actual figures on the mill test certificate, before using them for design or procurement.

Chemical & Mechanical

Properties by grade

Open a grade to see its nominal composition and typical mechanical properties.

Chemical composition (weight %) — Stainless Steel 304 / 304L
ElementContent
Chromium (Cr)18.0 – 20.0
Nickel (Ni)8.0 – 10.5
Manganese (Mn)2.0 max
Carbon (C)0.08 max (304) / 0.030 max (304L)
Mechanical properties (annealed) — Stainless Steel 304 / 304L
PropertyTypical value
Tensile strength515 MPa min
Yield strength (0.2 %)205 MPa min
Elongation35 % min
Density8.00 g/cm³

Chemical composition (weight %) — Stainless Steel 316 / 316L
ElementContent
Chromium (Cr)16.0 – 18.0
Nickel (Ni)10.0 – 14.0
Molybdenum (Mo)2.0 – 3.0
Manganese (Mn)2.0 max
Carbon (C)0.08 max (316) / 0.030 max (316L)
Mechanical properties (annealed) — Stainless Steel 316 / 316L
PropertyTypical value
Tensile strength515 MPa min
Yield strength (0.2 %)205 MPa min
Elongation35 % min
Density8.00 g/cm³

Chemical composition (weight %) — Cupro-Nickel 90/10 (C70600)
ElementContent
Copper (Cu)Remainder
Nickel (Ni)9.0 – 11.0
Iron (Fe)1.0 – 1.8
Manganese (Mn)1.0 max
Mechanical properties (annealed) — Cupro-Nickel 90/10 (C70600)
PropertyTypical value
Tensile strength275 MPa min
Yield strength (0.2 %)105 MPa min
Elongation30 % min
Density8.94 g/cm³

Chemical composition (weight %) — Cupro-Nickel 70/30 (C71500)
ElementContent
Copper (Cu)Remainder
Nickel (Ni)29.0 – 33.0
Iron (Fe)0.40 – 1.0
Manganese (Mn)1.0 max
Mechanical properties (annealed) — Cupro-Nickel 70/30 (C71500)
PropertyTypical value
Tensile strength370 MPa min
Yield strength (0.2 %)140 MPa min
Elongation30 % min
Density8.94 g/cm³

Chemical composition (weight %) — Copper (C11000 / C12200)
ElementContent
Copper (Cu)99.9 min
Phosphorus (P)0.015 – 0.040 (C12200)
OxygenTrace
Mechanical properties (annealed) — Copper (C11000 / C12200)
PropertyTypical value
Tensile strength205 MPa min
Yield strength (0.2 %)65 MPa min
Elongation40 % min
Density8.94 g/cm³

Chemical composition (weight %) — Inconel 625
ElementContent
Nickel (Ni)58.0 min
Chromium (Cr)20.0 – 23.0
Molybdenum (Mo)8.0 – 10.0
Niobium + Tantalum3.15 – 4.15
Iron (Fe)5.0 max
Carbon (C)0.10 max
Mechanical properties (annealed) — Inconel 625
PropertyTypical value
Tensile strength827 MPa min
Yield strength (0.2 %)414 MPa min
Elongation30 % min
Density8.44 g/cm³

Chemical composition (weight %) — Monel 400
ElementContent
Nickel (Ni)63.0 min
Copper (Cu)28.0 – 34.0
Iron (Fe)2.5 max
Manganese (Mn)2.0 max
Carbon (C)0.3 max
Silicon (Si)0.5 max
Sulphur (S)0.024 max
Mechanical properties (annealed) — Monel 400
PropertyTypical value
Tensile strength480 MPa min
Yield strength (0.2 %)170 MPa min
Elongation35 % min
Density8.80 g/cm³

Chemical composition (weight %) — Nickel 200 / 201
ElementContent
Nickel (Ni)99.0 min
Carbon (C)0.15 max (200) / 0.02 max (201)
Manganese (Mn)0.35 max
Iron (Fe)0.40 max
Silicon (Si)0.35 max
Copper (Cu)0.25 max
Mechanical properties (annealed) — Nickel 200 / 201
PropertyTypical value
Tensile strength380 MPa min
Yield strength (0.2 %)105 MPa min
Elongation40 % min
Density8.89 g/cm³

Chemical composition (weight %) — Aluminium 5083
ElementContent
Aluminium (Al)Remainder
Magnesium (Mg)4.0 – 4.9
Manganese (Mn)0.40 – 1.0
Chromium (Cr)0.05 – 0.25
Mechanical properties (annealed) — Aluminium 5083
PropertyTypical value
Tensile strength275 MPa min
Yield strength (0.2 %)125 MPa min
Elongation12 % min
Density2.66 g/cm³

Indicative data only. Values are typical for the grade and are shown for guidance. Confirm the applicable standard, and the actual figures on the mill test certificate, before using them for design or procurement.

Applications

Where it is used

Typical service environments for these materials.

Marine & Shipbuilding
Chemical Processing
Desalination
Heat Exchangers
Oil & Gas
Power Generation

Get in Touch

Tell us the grade and size

Rushabh Shah will come back to you directly with availability and pricing.